DC01, DC03 or DC04 Steel for Deep Drawing: Which Grade Should You Specify?
A frequent question from European buyers of formed steel parts, for example caps and cups produced in the thousands per year, is whether the quoted price is based on DC04 or on a cheaper grade. They ask because the grade changes how the part draws, what it costs, and whether a quotation from another supplier is comparable. This guide explains the three common grades, when to choose each and how to avoid a hidden grade change between quotation and production.
How DC01, DC03 and DC04 differ
| Grade | Typical use | What it means in the die |
|---|---|---|
| DC01 | Bent parts, brackets, shallow forming | Strongest of the three and least stretchy; fine for simple shapes, but it can tear at a tight corner of a deep cup |
| DC03 | Moderate draws, parts with some stretching | A step softer; a good middle choice when the draw depth is below the cup diameter |
| DC04 | Deep draws, tight radii, parts that will be drawn in more than one operation | Softer again, with more stretch before failure and a more uniform wall; the usual deep drawing steel |
EN 10130 sets maximum yield strength and minimum elongation for each grade, with the yield strength falling and the elongation rising from DC01 to DC03 to DC04. Check the current edition of the standard and the mill certificate for the exact limits that apply to your coil and thickness, because they also depend on the product form.
Choosing the grade by part shape
- Draw depth up to about half the diameter, generous corners: DC03 is normally enough, and DC01 can work for very shallow shapes.
- Draw depth around or beyond the diameter, small corner radius: specify DC04, and expect two or more draws with an intermediate anneal on the deepest parts.
- Parts drawn and then flanged, beaded or pierced: DC04 gives more margin because forming continues after the cup is made.
- Parts that must hold a flat face after forming: a stronger grade can be better, so tell us about flatness requirements.
Why the grade is a price lever and a comparison trap
The sheet price of a deeper-drawing grade is usually a little higher, so a supplier who is trying to hit a price may quietly quote a shallower-drawing grade. The result is often more scrap, an extra operation, or cracked corners in production. Ask each supplier to state the grade in the quotation and again on the material certificate. A recent request for formed steel parts with a yearly volume in the thousands per item was clarified on exactly this point: the buyer asked the supplier to confirm that both parts in the quotation were based on DC04, and the supplier confirmed it in writing.
What to write in the RFQ
- The grade (for example DC04), the thickness and its tolerance, and the surface finish required on the sheet.
- Drawing with the draw depth, the corner radii and the wall thickness requirement after drawing.
- Coating after forming, such as zinc plating, galvanizing or paint.
- First order quantity and annual quantity, because tooling and the number of draw stages depend on volume.
- Whether a mill certificate for the coil is needed, and whether the grade must be stated on it.
How we handle the grade
We work with steel grades to the standards your drawing names, and we state the grade on the quotation. Parts are produced through our production network across Guangdong, Zhejiang, Jiangsu, Shandong and Fujian. Our tolerance on stamped features is ±0.01 mm, and our largest drawn depth is 400 mm. If your drawing needs a grade we do not usually hold, we tell you in the first reply, together with any effect on lead time.
Frequently asked questions
Which steel grade should I choose for a deep drawn steel part?
DC04 is the usual choice for parts that are drawn deeply or have tight corner radii, DC03 for moderate draws, and DC01 for shallow forming and simple bent parts. A higher grade is softer and stretches more before it tears, so it lowers the risk of cracks at the corner. Ask the supplier to name the grade in the quotation.
Is DC04 more expensive than DC01?
The sheet price per kilogram is usually somewhat higher for the deeper-drawing grades, but the difference is small next to scrap, a second draw or a rejected lot. A deeper grade that avoids one extra draw or anneal step can lower the total cost of the part.
Can a quotation be compared if one supplier quotes DC04 and another DC01?
Not directly. Different grades behave differently in the die and are priced differently, so ask every supplier to quote the same grade, thickness tolerance and surface finish, and to write the grade on the quotation and on the material certificate.
How do I check the grade I receive?
Ask for a mill certificate for the coil used, stating the grade and the mechanical properties, and compare it with the grade in the order. Hardness checks on incoming sheet and a sample of finished parts are also useful.
Does the grade matter if the part will be galvanized or painted afterwards?
Yes, in two ways: the surface quality grade of the sheet affects how the coating looks, and a part that cracks or thins at a corner will fail first at that point. Mention the coating in the RFQ so the supplier can pick sheet with a suitable surface.
Send your drawing for a quote
Send the drawing with the steel grade, thickness, coating, first-lot and annual quantities and your delivery country. We reply with a quote and a DFM review within 24 hours.